The Specification For Lithium Nickel Manganese Cobalt Oxide
Lithium nickel manganese cobalt oxide NMC523 NCM532 powder for Lithium ion Battery Cathode Raw Material.
Product: |
Lithium Nickel Manganses Cobalt OxideLiNiMnCoO2 NMC532/NCM523 |
|
Ni:Mn:Co |
5: 3: 2 |
|
Application: |
High Capacity |
|
Term |
Standard |
|
Ni+Co+Mn (%) |
≥57.17 |
|
Li (%) |
7.00-8.00 |
|
H2O (%) |
≤0.1 |
|
D10 (µm) |
≥5.0 |
|
D50 (µm) |
8.0-12.0 |
|
D90 (µm) |
≤25.0 |
|
PH Value |
≤11.00 |
|
Pressed Density (g/cm3) |
≥2.20 |
|
Specific Surface Area (m2/g) |
0.30-0.80 |
|
Firstdischarge Capacity (mAh/g) |
≥155(0.2C,4.2-2.7V,Button half open cell) |
|
First Dischange efficiency(%) |
83-85% |
|
Appearance |
Black Powder、No Agglomeration、No Sundries |
|
Storage,Delivery |
Avoid moist |
|
Use Time |
One Year |
Exhibition
Cerificate